I ground the second run smooth to eliminate any little bits where it hadn’t quite filled properly.  You would normally do a 3 pass fillet on this now, but I didn't want to get the bead to close to the bolt holes, so I did just 2 runs instead.  Here I’m about half way round on the first run.  Even as it is I might have to grind a bit off to allow the bolt heads to fit properly as the bead ended up a bit closer than I would have liked.  I used E309L electrodes at 100 amps.  They are both ready for machining now.